Sorry, but Uniplate does not utilize palladium. I have their literature and
it specifically states NO palladium....rather it uses a conductive polymer
(non metal).... However, that aside, what I am more interested in is
feedback, anecdotal or otherwise, from those who have used it/ heard about
its pros/cons, know other who have used it, know of any other conductive
polymer process similar to Uniplate....
Dave
At 11:14 PM 5/18/99 +0100, Paul Brown wrote:
>The Uniplate process is a conductive polymer based on palladium as the final
>conductive layer
>The palladium is ionic and reduced to con the hole walls
>-----Original Message-----
>From: David Pizzoferrato <[log in to unmask]>
>To: [log in to unmask] <[log in to unmask]>
>Date: 18 May 1999 22:39
>Subject: Re: [TN] Conductive Polymer
>
>
>>No, I am not referring to screen printed conductive inks. What I am
>>referring is a replacement for electroless copper. A means by which to
>>sensitize the drilled hole wall in order to accept subsequent electroplate
>>copper. Specifically, conductive polymer process (Uniplate/Autotech) . Not
>>to be confused with carbon based "SHADOW" or "BLACK HOLE" technology.
>>
>>Regards
>>Dave
>>
>>
>>
>>At 10:07 PM 5/18/99 +0100, Paul Brown wrote:
>>>When you say conductive polymer do you mean screen printed conductive inks
>>>or palladium type processes
>>>at my last company we developed and installed a number of "direct plate
>>>installations " to replace electroless copper. This system was based on a
>>>reduced palladium conductive film, not a conductive organic layer
>>>Do you want more info
>>>Regards
>>>Paul Brown
>>>(UK 10pm, raining and cold (8'C))
>>>-----Original Message-----
>>>From: Fred S. Shubert <[log in to unmask]>
>>>To: [log in to unmask] <[log in to unmask]>
>>>Date: 18 May 1999 21:50
>>>Subject: Re: [TN] Conductive Polymer
>>>
>>>
>>>>I would be very interested in reading this paper. Could you possibly
>>>compact
>>>>it and send it via e-mail? Or would you send it to me at:
>>>>
>>>>Fred Shubert
>>>>Kester Solder
>>>>2105 60th. Ave. Dr. E.
>>>>Bradenton, FL. 34203
>>>>
>>>>If that is not possible please let me know where I can obtain a copy.
>>>>
>>>>----- Original Message -----
>>>>From: Jason Smith <[log in to unmask]>
>>>>To: <[log in to unmask]>
>>>>Sent: Tuesday, May 18, 1999 3:08 PM
>>>>Subject: Re: [TN] Conductive Polymer
>>>>
>>>>
>>>>> I wrote such a paper along those lines, but it's too big (due to
>>>graphics)
>>>>to
>>>>> send over net.
>>>>>
>>>>>
>>>>>
>>>>> [log in to unmask] on 05/18/99 12:50:09 PM
>>>>>
>>>>> Please respond to [log in to unmask]; Please respond
>>>to
>>>>> [log in to unmask]
>>>>>
>>>>> To: [log in to unmask]
>>>>> cc: (bcc: Jason Smith/Lex/Lexmark)
>>>>> Subject: [TN] Conductive Polymer
>>>>>
>>>>>
>>>>>
>>>>>
>>>>> Hi all,
>>>>>
>>>>> I am looking for commentary (pro and con) on conductive polymer as a
>>>>> replacement for electroless copper. (not to be confused with carbon
>based
>>>>> technology i.e. Shadow, Black Hole etc.)
>>>>>
>>>>> More specifically I am looking for feedback on Uniplate. Reliability,
>>>>> process robustness, general acceptance by assemblers/customers, I
>>>>> appreciate all comments.
>>>>>
>>>>> Regards,
>>>>> Dave Pizzoferrato
>>>>>
>>>>> ################################################################
>>>>> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
>>>1.8c
>>>>> ################################################################
>>>>> To subscribe/unsubscribe, send a message to [log in to unmask] with
>>>>following text
>>>>> in the body:
>>>>> To subscribe: SUBSCRIBE TechNet <your full name>
>>>>> To unsubscribe: SIGNOFF TechNet
>>>>> ################################################################
>>>>> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
>>>>section for
>>>>> additional information.
>>>>> For technical support contact Hugo Scaramuzza at [log in to unmask] or
>>>>847-509-9700
>>>>> ext.312
>>>>> ################################################################
>>>>>
>>>>> ################################################################
>>>>> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
>>>1.8c
>>>>> ################################################################
>>>>> To subscribe/unsubscribe, send a message to [log in to unmask] with
>>>>following text in the body:
>>>>> To subscribe: SUBSCRIBE TechNet <your full name>
>>>>> To unsubscribe: SIGNOFF TechNet
>>>>> ################################################################
>>>>> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
>>>>section for additional information.
>>>>> For technical support contact Hugo Scaramuzza at [log in to unmask] or
>>>>847-509-9700 ext.312
>>>>> ################################################################
>>>>>
>>>>>
>>>>
>>>>################################################################
>>>>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
>1.8c
>>>>################################################################
>>>>To subscribe/unsubscribe, send a message to [log in to unmask] with
>following
>>>text in the body:
>>>>To subscribe: SUBSCRIBE TechNet <your full name>
>>>>To unsubscribe: SIGNOFF TechNet
>>>>################################################################
>>>>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
>section
>>>for additional information.
>>>>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>>>847-509-9700 ext.312
>>>>################################################################
>>>>
>>>
>>>################################################################
>>>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>>>################################################################
>>>To subscribe/unsubscribe, send a message to [log in to unmask] with
>>following text in the body:
>>>To subscribe: SUBSCRIBE TechNet <your full name>
>>>To unsubscribe: SIGNOFF TechNet
>>>################################################################
>>>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
>>section for additional information.
>>>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>>847-509-9700 ext.312
>>>################################################################
>>>
>>
>>################################################################
>>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>>################################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>>To subscribe: SUBSCRIBE TechNet <your full name>
>>To unsubscribe: SIGNOFF TechNet
>>################################################################
>>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>>################################################################
>>
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|