TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 1 May 2009 10:07:20 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Subject:
From:
"Kane, Amol (349)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (135 lines)
We have seen this exact phenomenon (as depicted in pics 2, 3 and 4, though not as acute as the one depicted in pic 1) on thermally challenging LF BGA board. The culprit is a combination of too little flux in the solder deposit (due to the deposit size) and too long soak. The little flux that's in the deposit burns off during the soak and the oxide layer on the solder sphere does not allow them to coalesce and dissolve in the bulk solder. In our case we could minimize it by reducing the soak on the profile







-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Parsons
Sent: Thursday, April 23, 2009 2:16 PM
To: [log in to unmask]
Subject: [TN] Solder Ball Problem



I am trying to get to the root of a little solder ball problem.  The problem

is specific to a single part and was evident on the first run of this board

a few months ago.  We are seeing it again on this run although the common

denominator here is that the PCB's are all from the same production batch.



It appears that the formation of solder balls can be reduced by pre-baking

the PCB's (100°C for 4-8 hrs) but not eliminated.  The best results are

obtained by pre-conditioning the PCB's by running them through the reflow

oven first,  letting them cool, then print, populate and re-flow.  The

majority of balls now formed are dealt with at wash.



The PCB's are simple double sided, HASL finish.  I suspect a problem with

the solder finish (HASL) but what exactly that "problem" is I am not sure.

FYI, paste is water soluble.



http://stevezeva.homestead.com/files/Solder_ball_1.jpg - this photo is of a

board that was pre-baked for about 4 hours @ 100°C, it was then printed and

re-flowed.  It does not matter if the 4 hour bake improved things you can

see that the results are pretty spectacular.



The following pictures are really more of the same except that these boards

have been populated and washed.



http://stevezeva.homestead.com/files/Solder_ball_2.jpg



http://stevezeva.homestead.com/files/Solder_ball_3.jpg



http://stevezeva.homestead.com/files/Solder_ball_4.jpg



Any insight would be appreciated.



(thanks to Steve for hosting the photos)



Regards

John Parsons



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------



WARNING:  Export Control 
This document may contain technical data within the definition of the 
International Traffic in Arms Regulations (ITAR), and subject to the Export 
Control Laws of the U.S. Government.  Transfer of such data by any means to a 
foreign person, whether in the United States or abroad, without proper export 
authorization or other approval from the U.S. Department of State is 
prohibited. 
 
CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy 
all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2