TECHNET Archives

June 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 19 Jun 2007 17:34:15 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Joe Fjelstad <[log in to unmask]>
Parts/Attachments:
text/plain (51 lines)
 
Thanks Richard. 
 

I like your analogy, though when you mentioned it my thoughts ran to carp  
the boniest fish I have ever encountered. 
 
The fishbone diagram reference was not from me but from Ingemar  Hernefjord. 
It is impressive. 
 
Best, 
Joe  

 
In a message dated 6/19/2007 2:22:57 PM Pacific Daylight Time,  
[log in to unmask] writes:

Hi,  Joe
I don't believe I have ever seen the fishbone charts that you  describe,
but I do know that Electrovert has a similar chart for  determining the
root cause(s) of wave soldering defects.
And the  IPC-HDBK-001 has Tables that used to be wishbone charts for
individual  processes, such as Table 7-4 (Common printing problems),
Table 7-9 (VPS  problems/solutions), etc, that could become individual
branches on the  fish.

I think a lot of us are just waiting for the same answer as you;  we
would all love to see a wishbone chart by which we can trace back  the
possible cause for a given assembly or solder defect.

But this  particular wishbone chart, if it even exists, would have more
individual  bones than a Minnesota Northern Pike. 







************************************** See what's free at http://www.aol.com.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2