TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 9 Jan 2006 11:52:56 -0500
Reply-To:
Subject:
From:
Kevin Glidden <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
Organization:
LSI
MIME-Version:
1.0
Parts/Attachments:
text/plain (23 lines)
Hello Technetters - Happy Monday.

Does anyone have experience using swaged hardware (specifically A-A-51926/29
swage mount turret terminals) on aluminum MCPCBs (Metal-Core Printed Circuit
Boards)?  I know swaged terminals are routinely used on traditional FR4
boards, but is there a concern of z-axis thermal expansion on the aluminum
MCPCB putting too much strain on the plated-thru holes with the swaged
terminals installed?  I would like to use the swage mount terminals to avoid
the hand soldering of terminals on thh MCPCB, with an .040" aluminum core
and total PCB thickness = .110 +/- .010

Thanks in advance.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2