TECHNET Archives

September 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 18 Sep 2012 18:50:08 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
<0F07EE77FE883741A9A0B3B7DCD9368202DD80E4@phoxcg01>
Subject:
From:
John Foster <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (58 lines)
The highest voltage we will see is +5v. So you feel it's an electrical
isolation issue?
Thanks

-----Original Message-----
From: Joyce Koo [mailto:[log in to unmask]] 
Sent: Tuesday, September 18, 2012 6:10 PM
To: [log in to unmask]; Foster, John @ CSG - PHOTONICS
Subject: Re: [TN] question about 6012

What voltage of your application?  Some of hid operated at blow 4v. 1.8
are common.  If you are working on 18v, I would be a bit of worry. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: John Foster [mailto:[log in to unmask]]
Sent: Tuesday, September 18, 2012 09:03 PM
To: [log in to unmask] <[log in to unmask]>
Subject: [TN] question about 6012

I am curious about the 3.543 uin dielectric spacing recommendation in
6012C 3.6.2.15. I have to believe that this

Number did not just come out of thin air. I have been searching for any
long term reliability issues related to going below this number. I know
that HDI structures and embedded capacitors use very thin dielectrics
and the spec recommends low profile copper when going below this number.
We are doing Class 3 boards  and I am just trying to make sure I am not
shooting myself in the head going below this number. 

Thanks in advance


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2