Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Date:
Thu, 10 Apr 2008 06:59:44 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Sauer, Steve (Xetron)" <[log in to unmask]>
Subject:
From:
"Sauer, Steve (Xetron)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (85 lines)
The connector is ~ 2.5" long (3 banks of 16 pin pairs per side).
The PCB is 6 layer construction using FR-406.
Thanks for your input.

Steve  

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Wednesday, April 09, 2008 5:16 PM
To: [log in to unmask]
Subject: Re: [TN] Samtec QMSS-DP Series Differential Pair Connectors

How long is the connector?. It is far more likely you have a connector /
board coplanarity issue.

John

 
 
John Burke
 
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Sauer, Steve
(Xetron)
Sent: Wednesday, April 09, 2008 11:24 AM
To: [log in to unmask]
Subject: [TN] Samtec QMSS-DP Series Differential Pair Connectors

Good Afternoon,
Does anyone have any experience with the subject connectors?
I'm currently evaluating these connectors (the mate is QFSS series) for
a new application and am experiencing issues with coplanarity of the
leads resulting in random nonsoldered pins.  The coplanarity is listed
on the spec sheet as .004" (.10mm) max and I'm using a 6mil stencil with
1:1 apertures (as recommended by the mfr).
Thanks in advance for your assistance.

Steve

Steve Sauer, CEPM
Sr. Project Engineer
Northrop Grumman Xetron
Cincinnati, OH
513-881-3368
[log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2