I got some good feedback from a couple of engineers working over the weekend
and have produced some more images to show "Fisheyes" now. I will reliable
the first examples circulated as "BugEyes" as they remind me of the VV
Beatle.
I did find a reference to FishEyes in a NASA standard with a black and white
photo. There is also a colour image in their inspection guide.
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
New Bob Willis "Printed Board Inspection & Quality Control Workshop" 24th
March www.ASKbobwillis.com/faworkshops.pdf
"Troubleshooting Your Assembly Yields Workshop" 25th March
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 22nd April
www.ASKbobwillis.com/faworkshops.pdf
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey (EHCOE)
Sent: 23 February 2009 16:15
To: [log in to unmask]
Subject: Re: [TN] Conformal Coating Inspection
In regards to plated-through holes, it would probably be Walleyes.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Willis
Sent: Friday, February 20, 2009 8:52 AM
To: [log in to unmask]
Subject: [TN] Conformal Coating Inspection
I have been putting together some inspection standards for a new
workshop in
Germany. I have found a number of references to "Fish Eyes" but never
seen
an example. It's a common term but seems to be elusive in terms of
actual
examples.
Would the images at the following link be considered "Fish Eyes" by
users or
are we looking for more subtle examples like two bubbles between IC
leads??
www.ASKbobwillis.com/gonefishing.pdf
Many thanks
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
New Bob Willis "Printed Board Inspection & Quality Control Workshop"
24th
March www.ASKbobwillis.com/faworkshops.pdf
"Troubleshooting Your Assembly Yields Workshop" 25th March
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 22nd April
www.ASKbobwillis.com/faworkshops.pdf
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|