> Good evening Kelly,
> (you must be working near the east coast, arent you?)
>
> Top 1:
> are these major effects on the soldering process still true, if this the
> insert is only about 2x3 mm2 ?
>
> Your new process, how does it deal with the huge tolerances? Can you tell
> more about it?
> In my processes, I can not allow to get large forces on my IC-package
> during mountig of the heat sink. Thats the reason why i think of having
> the insert preassembled before SMT Placement and reflow.
>
> Using an adhesive (even with l=8W/mK) is a "week" solution compare to
> copper.
>
> Top 2:
> why not use copper? the PCB is adjusted to lie somewhere between copper
> and silicon
> how expensive is the assembly, any estimate compared to standard FR4
> double side?
>
> who does manufacters such things?
>
> BTW: what does SCI manufactures?
>
> Regards - Wolfgang
>
>
>
> ----------
> Von:
> [log in to unmask][SMTP:[log in to unmask]]
> Gesendet: Montag, 12. Oktober 1998 14:57
> An: [log in to unmask]
> Betreff: RE:[TN] Inserts into PWB
>
>
> Good morning Wolfgang -
>
> Yes, quite a few of us use "thermal cores" with our circuit boards.
> We have
> at various times used aluminum, alumina, copper and graphite. All
> of these
> items can be very efficient heat sinks. A few words of caution, in
> a
> practical sense:
>
> 1] Addition of an efficient heatsink, can and will have a major
> effect on your
> soldering process. Accordingly, we try to design a structure that
> will allow
> addition of the heatsink AFTER the soldering process has been
> completed;
> 2] Bonding the heat sink to a circuit board will make the circuit
> board try to
> emulate the expansion of the heat sink UNLESS a compliant adhesive
> is used to
> mechanically decouple the two.
> 3] Be careful to ensure that the bond line provides sufficient
> dielectric
> spacing to prevent shorting from the cirucuit board to thermal core.
>
> While it is possible to laminate a predrilled, filled sheet of
> aluminum or
> copper into the basic circuit board, I do not recommend this
> practice for the
> reasons noted above.
>
> Regards - Kelly
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|