With regards to Peters suggestion of silver deposition, I had suggested that
to them and I will mention it again.
Eric, your questions are all good, but I do not have that information at
this time. Is your organization in such things? Should I hook up my
customer with you directly?
John
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric CHRISTISON
Sent: Friday, March 04, 2005 8:34 AM
To: [log in to unmask]
Subject: Re: [TN] Conductive Pattern on Lexan?
How big a component are they talking about and is it flat or 3 dimensional?
Do they need good adhesion? What sort of environment is this part destined
for?
Regards,
Eric Christison
Mechanical Engineer
Consumer & Micro Group - Imaging Division
STMicroelectronics
33 Pinkhill
Edinburgh
EH12 7BF
Tel: +44 (0)131 336 6165
Fax: +44 (0)131 336 6001
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
> Sent: Friday, March 04, 2005 4:21 PM
> To: [log in to unmask]
> Subject: Re: [TN] Conductive Pattern on Lexan?
>
>
> Lexan is GE's generic trade name for their polycarbonate
> resin family, so there are various grades, probably one would
> be OK. A flex circuit manufacturer would be a good place to
> start talking as it is likely to be similar process to those
> used to make polymer circuitry.
>
> Regards
>
> Mike Fenner
> Indium Corporation
>
> T: + 44 1908 580 400
> M: + 44 7810 526 317
> F: + 44 1908 580 411
> E: [log in to unmask]
> W: www.indium.com
> Pb-free: www.Pb-Free.com
>
>
>
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of John Parsons
> Sent: Friday, March 04, 2005 4:00 PM
> To: [log in to unmask]
> Subject: [TN] Conductive Pattern on Lexan?
>
>
> Happy Friday!
>
>
>
> I have a customer who would like to produce a conductive
> pattern, preferable with a gold finish on ½ to 1” thick Lexan
> or some other clear dielectric. Clear because they want to be
> able to see through it and the thickness will be required to
> withstand a significant pressure that will be on the surface.
> That is all the information I have at present.
>
>
>
> Any of you guru’s out there have any ideas/suggestions as to
> either the feasibility or impossibility? Offhand I don’t
> know if Lexan would stand up to the various processes in the
> regular PCB etching/plating processes. Even suggestions as
> to another industry capable of this feat would be appreciated.
>
>
>
> Regards
>
> John Parsons
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV
> 1.8e To unsubscribe, send a message to [log in to unmask] with
> following text in the BODY (NOT the subject field): SIGNOFF
> Technet To temporarily halt or (re-start) delivery of Technet
> send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
:::::::::::::::::::::::::::
This email, its content and any files transmitted with it are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient please delete and
contact the sender by return and delete the material from any computer. Any
review, retransmission, dissemination or other use of, or taking of any
action in reliance upon, this information by persons or entities other than
the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness. In particular, Indium
Corporation does not accept responsibility for changes made to this email
after it was sent. Any opinions or recommendations expressed herein are
solely those of the author. They may be subject to change without notice.
:::::::::::::::::::::::::::
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|