Hi Dan,
Don't know where you are located, but I believe Six
Sigma in Milpitas California has pre-tin service. You
can reach them at 408-956-0100 or go to
www.sixsigmaservices.com
Ted
--- "Dan R. Johnson" <[log in to unmask]> wrote:
> I have a customer requirement to pre-tin the leads
> on some of our parts. The
> part is a TO-8 header. The requirement is that only
> the last .05" +/- .015"
> of the lead be tinned. I will have a drawing
> available later today.
> Does anyone provide this service or know of a
> source?
>
> Thanks,
> Dan
> BTW; Given recent threads replies should probably be
> off line ;)
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC
> using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
>
-----------------------------------------------------
__________________________________
Do you Yahoo!?
Yahoo! Calendar - Free online calendar with sync to Outlook(TM).
http://calendar.yahoo.com
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------