Chuck,
What David Whalley was refering to is a in line Plasma Cleaning Machine called ITRAK by
MARCH Instruments (Advance Packaging, February 2000). Tel. 925-827-1240, or
www.nordsonplasma.com. It is coveyorised per the picture in the ad.
Chuck Brummer wrote:
> Hi Techies,
>
> About ten years ago I saw a conveyorized plasma clean unit at NEPCON.
> It was small and used an oxygen plasma to clean substrate surfaces. It
> had an entrance and exit lock to help with the vacuum and a main chamber
> for the plasma reaction. Does anyone else remember this equipment? I
> would like to find one if they still exist. It's OK if your a
> salesperson (PC).
>
> Chuck Brummer
> [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
--
____________________________________
Regards,
Pratap Singh
Tel./Fax: 512-255-6820,
e-mail: [log in to unmask] or [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|