TECHNET Archives

January 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
jckim(김정철) <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, jckim(김정철) <[log in to unmask]>
Date:
Thu, 29 Jan 2009 16:40:54 +0900
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)


Hello Techneters,



I want to know why do we have to do e'lytic Ni/Au plating on tab pad of memory module PCBs.

I mean why specified surface finish and why specified 'gold' thickness.

(mostly specified by set makers. Industry standards like IPC and JEDEC seems to just recommends.) 



If Ni/Au plating with reduced thickness or other finishes can meet mechanical/reliability requirement in their socketing application,

isn't it okay to use?



Is there any siginificant reason in using e'lytic Ni/Au plating with specified thickness??



Thanks for the kind answer in advance.

Good day!



jc