Hi Carl,
As XRF analyzes relatively deep layers, one can not tell where As could be coming from. You'd have to do proper analysis to establish the root cause for the problem.
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: Carl Ray <[log in to unmask]>
Date: Tue, 8 Jun 2010 11:44:21
To: <[log in to unmask]>
Subject: [TN] Arsenic from XRF Testing
All,
I have a question. We were seeing some solderability issues with some components that were provided by our customer. These devices were Sn-Pb over Cu plating per the data sheet. We tested 3 samples and noticed where all three samples have very high concentration of Arsenic. Some as much 4-5%. What could possibly be the cause for this? I understand Arsenic is used during plating process but I did not think it was as significant as 4-5%.
Carl Ray
Staff Engineer
Teledyne Electronic Manufacturing Services
1425 Higgs Rd.
Lewisburg, TN 37091
Direct: 931-270-2724
Cell: 931-637-5958
Email: [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|