TECHNET Archives

April 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"McMonagle, Mike" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 27 Apr 2000 09:11:02 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (70 lines)
Craig,
        See IPC-A-610B Rev B, Section 4.2.1, 'Exposed Basis Metal'. There is
a note that addresses OSP and exposed copper. Even without applying the
note, it is still considered only a process indicator rather than a
nonconforming defect.

        If you are already working to the new release of IPC-A-610C, it is
covered in better detail in Section 6.5.2, 'Exposed Basis Metal'.

Mike McMonagle
PCBA Process Engineering
Telxon Corporation
(713) 307-2443 Phone
(713) 307-2581 Fax
www.telxon.com

' Innovative Solutions for
Mobile Information and
Wireless Communications'


-----Original Message-----
From: Craig Leppanen [mailto:[log in to unmask]]
Sent: Thursday, April 27, 2000 7:47 AM
To: [log in to unmask]
Subject: [TN] spec for exposed copper


All-

I have a situation on an SMT OSP board.  There is some exposed copper on the
periphery of fine pitch lands.  The lands have greater than 85% solder
coverage
and acceptable joints.  But the customer is concerned about the exposed
copper.
I have not seen a spec explicitly stating that exposed copper on an OSP
board is
acceptable.  Does such a spec exist??

Thanks, Craig Leppanen

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2