Dennis Fritz <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 24 Jul 2009 16:10:48 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (313 lines)
Now this is the Purdue Technology Center Summer Intern "patent-pending" ?inspection device for tin whiskers. Steve, please post to your web site for IPC pictures.? Here is the link to Ebay for more of these $50 digital microscopes. Remember, there is no vernier on here to measure distance. 

Also, the price went to $49.99!!!






New 1.3 Mega Pixel USB Digital Microscope 230x Zoom A3 

8 LED Light,inspect Stamps, currency, jewelry,Skin,etc.








Item condition:

New

























Quantity:






More than 10 available


Please enter a quantity of $quantity$ or less 
Please enter a quantity of 1








Price:

US $66.66US $49.99


Sale ends in 3 days
Buy It NowBuy It Now









You can also:

Watch this item





Now watching in My eBay 



















Shipping:

FREE shipping?Standard Flat Rate Shipping ServiceSee more services?See discounts??|? See all details 
Estimated delivery time varies for this shipping service. Seller ships within 1 day 








Returns:






14 day?money back,?buyer pays return shipping?| Read details










Link. 
http://cgi.ebay.com/New-1-3-Mega-Pixel-USB-Digital-Microscope-230x-Zoom-A3_W0QQitemZ280372533230QQcmdZViewItemQQptZLH_DefaultDomain_0?hash=item41478157ee&_trksid=p3286.c0.m14&_trkparms=65%3A12%7C66%3A2%7C39%3A1%7C72%3A1205%7C293%3A1%7C294%3A50


-----Original Message-----
From: Dennis Fritz <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, Jul 24, 2009 3:13 pm
Subject: Re: [TN] PCB Inspection - with added E-bay "digital microscope"



Ken, 

Just catching up on this discussion.?We have college interns checking for tin 
whiskers on commercial electronics.? I just bought one of these "digital 
microscopes" on E-bay for $40.? For that kind of money how can you go wrong?? 
Well ........

1. The little unit is easy to hook to your computer and the software is pretty 
good for image capture.? There is a good white LED illuminator around the camera 
lens.? I think the application is more for detecting counterfeit money, as the 
little camera does magnify the maximum 230X and take decent pictures, but it 
works best on flat surfaces.? 

2. Nothing works like a microscope stage to smoothly move objects in the X-Y 
directions so you can scan.? There is no Z-axis movement except to bring the 
object closer or further away, The camera goes in and out of focus to drive you 
crazy. 

3. We mounted our $40 scope to our metallurgical microscope and use it that 
way.? It makes the cheapest digital add-on I have seen to an existing optical 
microscope!!!? And you can't beat the price or ease of set-up.? 

Contact me off line and I will send a picture of how we use it here at Purdue 
Techology Center. 

Denny Fritz


-----Original Message-----
From: Leif Erik Laerum <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, Jul 24, 2009 11:31 am
Subject: Re: [TN] PCB Inspection


Kenneth,?
?
I have two of these. I never use them for anything. The image quality is 
unsuitable for detecting PCB blemishes. We use Mantis Scopes with 10X 
magnification. We catch everything with that. Different price class of course.?
?
Leif Erik Laerum?
?
?
Kenneth Wood wrote:?
> As I've said in the past...this list server really needs to support HTML?
> format...?
> Let's try this again.?
>?
> https://webvia.techni-tool.com/VIA/viaImagePageIndex.jsp?row=17&pgName=viaLi?
> stProducts.jsp&searchText=IN6&modifier=IN6&reqTitle=TITLE_VIAUSERDOCLIST&new?
> Window=Y?
>?
>?
> If this still doesn't work, please go to www.techni-tool.com and look up?
> part number 876IN414?
>?
> Thanks?
> Ke
n?
>?
>?
>?
> -----Original Message-----?
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Kenneth Wood?
> Sent: Friday, July 24, 2009 10:09 AM?
> To: [log in to unmask]
> Subject: [TN] PCB Inspection?
>?
> Hi all..?
>?
> I need to inspect a small lot of bare boards and was wondering if anyone had?
> experience with this unit:?
>?
> >?
> https://webvia.techni-tool.com/VIA/viaImagePageIndex.jsp?row=17?
> <https://webvia.techni-tool.com/VIA/viaImagePageIndex.jsp?row=17&pgName=viaL?
> istProducts.jsp&searchText=IN6&modifier=IN6&reqTitle=TITLE_VIAUSERDOCLIST&ne?
> wWindow=Y>?
> &pgName=viaListProducts.jsp&searchText=IN6&modifier=IN6&reqTitle=TITLE_VIAUS?
> ERDOCLIST&newWindow=Y?
>?
> >?
> Or.is there something better I can use to perform a visual inspection of?
> bare boards??
> Thanks?
>?
> Ken?
>?
> >?
>?
> ---------------------------------------------------?
> Technet Mail List provided as a service by IPC using LISTSERV 15.0?
> To unsubscribe, send a message to [log in to unmask] with following text in?
> the BODY (NOT the subject field): SIGNOFF Technet?
> To temporarily halt or (re-start) delivery of Technet send e-mail to?
> [log in to unmask]: SET Technet NOMAIL or (MAIL)?
> To receive ONE mailing per day of all the posts: send e-mail to?
> [log in to unmask]: SET Technet Digest?
> Search the archives of previous posts at: http://listserv.ipc.org/archives?
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16?
> for additional information, or contact Keach Sasamori at [log in to unmask] or?
> 847-615-7100 ext.2815?
> -----------------------------------------------------?
>?
> ---------------------------------------------------?
> Technet Mail List provided as a service by IPC using LISTSERV 15.0?
> To unsubscribe, send a message to [log in to unmask] with following text in?
> the BODY (NOT the subject field): SIGNOFF Technet?
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)?
> To receive ONE mailing per day of all the posts: 
send e-mail to 
[log in to unmask]: SET Technet Digest?
> Search the archives of previous posts at: http://listserv.ipc.org/archives?
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815?
> -----------------------------------------------------?
> ?
---------------------------------------------------?
Technet Mail List provided as a service by IPC using LISTSERV 15.0?
To unsubscribe, send a message to [log in to unmask] with following text in?
the BODY (NOT the subject field): SIGNOFF Technet?
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)?
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest?
Search the archives of previous posts at: http://listserv.ipc.org/archives?
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815?
-----------------------------------------------------?


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2