Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Wed, 20 Nov 1996 07:45:00 -0600 |
Precedence: |
list |
Resent-From: |
|
From [log in to unmask] Wed Nov 20 09: |
01:21 1996 |
Resent-Sender: |
|
Content-Transfer-Encoding: |
7bit |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
Resent-Message-ID: |
<"EpSlL1.0.B8O.KXnao"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vQDpC-0000XkC; Wed, 20 Nov 96 08:40 CST |
X-Mailer: |
Microsoft Exchange Server Internet Mail Connector Version 4.0.993.5 |
Message-Id: |
|
Parts/Attachments: |
|
|
I don't know if this helps for PCBs but Kapton is a UL recognized
material. It is in the 1996 Plastics Recognized Components Directory on
page 128.
----------
From: KoizumiT
To: [log in to unmask]
Subject: Why Polyimide is Not ANSI?
Date: Wednesday, November 20, 1996 2:25AM
Dear TechNetters:
I am wondering why Polyimide Film materials such as Kapton,
Apical,
Upilex etc. are not recognized as a same ANSI grade although these
PI
films have very similar molecular formula and properties.
As we are manufacturing Flexible Printed Circuits using these
materials, our UL application is very complexed because they are
not
recognized as ANSI.
Does anyone trying to set up ANSI grade for polyimide films in
use
of FPC? Or does anyone knows suitable forums for this discussion?
Best Regards,
Toru Koizumi(Mr)
Fujikura Ltd. Japan
[log in to unmask]
************************************************************************
***
* TechNet mail list is provided as a service by IPC using SmartList
v3.05 *
************************************************************************
***
* To unsubscribe from this list at any time, send a message to:
*
* [log in to unmask] with <subject: unsubscribe> and no text.
*
************************************************************************
***
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|