TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0voCcH-0000SBC; Sat, 25 Jan 97 12:14 CST
Old-Return-Path:
Date:
Sat, 25 Jan 1997 10:22:24 -0800
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9635
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"Mqq1z.0.qMM.rrawo"@ipc>
Subject:
From:
Bob Metcalf <[log in to unmask]>
Message-Id:
X-Loop:
X-Mailer:
Novell GroupWise 4.1
From [log in to unmask] Mon Jan 27 08:
40:22 1997
Parts/Attachments:
text/plain (27 lines)
John, LPI solder mask's do contain fillers that make the mask less than
"crystal clear" when using so called "clear" versions. Perhaps a more
appropriate name for these masks would be "colorless". 

I'm not sure why you were told the mask would go "clear" after wave
solder. That would not be my expectation. To insure we are talking about
the same thing, I would suggest you send me a sample of what you are
seeing. 

Please feel free to contact me at: 714-730-8356

Regards,
Bob Metcalf
Morton Electronic Materials

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2