TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 20 Nov 2008 13:44:29 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ted Tontis <[log in to unmask]>
Subject:
From:
Ted Tontis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<9C08C8377CA543719456E8F306C72549@ingemar2a39615>
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (28 lines)
The current company I work for works mostly with automotive LED lighting as
well as indoor and outdoor LED lighting. Large portions of the LED's we deal
with are three or four dollars a piece, so scrap is not something we take
lightly. What we have found useful is to have a special training program for
repair and cell operators. We focus on correct hand soldering, component
removal and solder joint repair of the LED's. During the hands on training
session we attach thermocouples to the dies and leads of the LED's and
attach them to a data logger. This helps train the operator on the correct
time and temperature needed to repair an assembly without damaging the LED
but still have an adequate solder joint. We also add the information to the
process sheets and lock the temperature adjustments. In one application we
plow air on the dome of the LED to keep the die from being damaged. Since
the implementation of the program our scrap rates have gone down
tremendously.


Ted T. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2