Hi Joe,
In a 3-parameter Weibull distribution, the third parameter is typically a
failure-free period. While a good case can be made for a failure-free period
based on physics-of-failure arguments, typically not enough of a
statistically robust data base is generated to allow an evaluation of an
appropriate failure-free period. I there fore do not use one to err, if at
all, on the side of conservatism.
The fatigue life of plated-through-vias in IPC-TR-579 has been updated to
include the effects of stress concentrations (see IPC-D-279) and has been
further modified based on the results witth polyimide PWBs.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|