Chris,
Your req for 0.020" max is very tight indeed, I can see more
serious problem of solder joint fractures with shaving off board
surfaces.
I think IPC610 specifies min 0.040", being 0.060" is typical.
Check section 3 or 4. I don't think you can get repeatable
process with the tight requirement. Remember boards get
warped one way and another after wavesoldering.
Some of things you can do; - provide more support pins, so
boards stays even during leadtrimming, - move the trimming
blade at a constant and controlled speed (slower is better), -
avoid cutting heavy leads, - use a new blade when you see a first
sign of flagging and bending of leads being cut.
regards
Matthew
NII, Norsat
>>> Chris_Smith <[log in to unmask]> July 16, 1998 11:39
am >>>
All,
I have a lead trim operation that uses a Q-corporation LOM II
trimming system with a vacuum fixture. We are using the
standard
cutting rings with a 30 degree angle. The Vacuum fixture
being used
is quite snug and there is very little vacuum loss in the
process.
The issue I have is the height requirement we're trying to
meet is
.020" max length. This strict requirement is resulting in pcbs
being
cut into and damaged, some flagging, and some solder
fractures. This
seems to be a very operator dependent operation and costly if
not done
correctly. I have tried varying the speed the cutter is moved
across
the board, having Q-corp sharpen the blades instead of us
doing it and
using a QB-1 PCB brusher which was purchased for this
product.
Is there anyone out there with a similar trim height
requirement
and what types of things do you perform to insure a
repeatable
process? Also anyone with suggestions please let me, I
need to get
this resolved if at all possible.
Thanks
Chris Smith
Manufacturing Engineer
################################################################
TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line
Services" section for additional information.
For technical support contact Hugo Scaramuzza at
[log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|