Steve,
If you don't mind a two part material, good old H20E from Epoxy
Technology Inc. (Epo-tek) is by far the most robust material I have used
to date. Resistively is spec'd at >.0004 ohm-cm.
Bill C.
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Wednesday, December 05, 2001 10:00 AM
To: [log in to unmask]
Subject: [TN] Conductive epoxy..
Hi All!!
I was wondering if anybody knows of a good silver filled liquid
conductive epoxy that has the same sort of conductivy as that of
Ablefilm 5025E...I'm gonna do some searching myself, but I thought that
I'd ask the experts first...
Thanks!
-Steve Gregory-