Hello Technet,
A question came up this morning as to whether nitrogen could be used as a
drying agent for PWBs, components, etc. I know nitrogen is used as a fill
gas for dry boxes, bags and to provide a dry atmosphere for component
testing. I don't have a feel for the physics of using nitrogen to dry
something out. We have a situation where baking at high temperatures may
not be practical but immersion in a nitrogen atmosphere is. Any ideas,
references would be appreciated.
Thanks,
Gregg
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------