Hi Wayne - I recommend you determine just how much flux and/or flux
residue remains under the component after processing. Your solvent
cleaning process may not be removing all or enough flux residue to allow
for the specific pwa circuit to function in a high humidity environment.
Carefully, without using flux, remove several other capacitors in that
region to see what is underneath. In some high humidity environments,
conformal coating is necessary due to circuit spacing and functionality.
Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Thayer, Wayne" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/26/2009 09:01 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Thayer, Wayne" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] humidity test failure
Hi Technet Gurus!
I have attached a picture of a part responsible for excess current draw
during an extended humidity/temperature cycling test. (I copied Steve so
he can hopefully post!)
The board was carefully solvent cleaned, but no SIR test validating the
process strips all ionic contamination. The board is in an enclosure
where plenty of ionic contaminants are available.
Humidity was supposed to not exceed 90% and was to be non-condensing
during cycling. There were a handful of components which displayed
similar deposits on the same circuit board. These were the only parts
biased during the humidity test. I believe the evidence suggests at least
some condensation occurred. To me the deposits look like salts. But
what do "the experts" think?
Is there any rule of thumb as to humidity levels where we are nuts to try
to survive without conformal coating? Part of the adjacent circuitry
contains RF devices and those guys get panic-stricken when told we
probably need to conformal coat!
Wayne Thayer
This e-mail and any files transmitted with it may be proprietary and are
intended solely for the use of the individual or entity to whom they are
addressed. If you have received this e-mail in error please notify the
sender.
Please note that any views or opinions presented in this e-mail are solely
those of the author and do not necessarily represent those of ITT
Corporation. The recipient should check this e-mail and any attachments
for the presence of viruses. ITT accepts no liability for any damage
caused by any virus transmitted by this e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|