In TSOP packages it can make your life miserable.  We had some memory
modules that gave us fits until the vendor finally switched over to a
Copper lead frame.  If you look at the technet archives, you will find a
huge discussion on this issue.
 ----------
From: Gabriela Bogdan
To: [log in to unmask]
Subject: ALLOY 42
Date: Friday, July 18, 1997 2:35PM


Hi, TechNetters !
I am alive and still hoping to get comments on Alloy 42 concerning the
quality
of solder joints ,pro and con's,if possible.I sent a message a week ago.

I wish to have sent a question about wedge voids too, but learned a lot
about
it ,unexpectedly.
Thank you all,
Gaby
P.S.:I have 2 e-mails:
[log in to unmask]
[log in to unmask]

************************************************************************
***
* TechNet mail list is provided as a service by IPC using SmartList
v3.05 *
************************************************************************
***
* To subscribe/unsubscribe send a message <to: [log in to unmask]>
 *
* with <subject: subscribe/unsubscribe> and no text in the body.
 *
************************************************************************
***
* If you are having a problem with the IPC TechNet forum please contact
 *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]
 *
************************************************************************
***

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2