Lyon, plastic blistering in a DIMM connector caused by solder process can be attributed to several possible causes including a housing material that is hygroscopic so may have absorbed excess moisture, it could be material with inadequate high temp resistance, improper molding, to name a few. What type of spec would you expect to see from IPC? JEDEC controls the DIMM modules and connector performance.
Jim McGrath
Strategic Marketing Manager
TE Consumer Devices
Cell: 630-244-3872
Email: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of LyonYuan
Sent: Tuesday, June 03, 2014 7:06 AM
To: [log in to unmask]
Subject: [TN] Have IPC standard can cover DIMM connector with blister after wave solder?
Guys
Have IPC standard can cover DIMM connector with blister after wave solder?
Lyon Yuan
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|