Brs,
What is the likelihood that the woven glass cloth had some spots/areas which did not accept the treatment process. I believe that the term for this is resin recession, non-wetting. Is it possible that this anomaly could cause an exothermic event to occur?
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerry Gagnon
Sent: Wednesday, September 25, 2013 2:09 PM
To: [log in to unmask]
Subject: Re: [TN] PWB / PCB fabrication
Hi Victor,
Treatments for the different resin types are typically applied by the glass fiber/glass cloth manufacturer.
Brs,
Gerry Ggnon
> Date: Wed, 25 Sep 2013 10:45:15 -0500
> From: [log in to unmask]
> Subject: [TN] PWB / PCB fabrication
> To: [log in to unmask]
>
> Fellow TechNetters;
>
> When is the glass woven cloth condition to accept the resin for laminate bonding? Is this a portion of the fab process or is the vendor of the woven glass cloth condition by the vendor?
>
>
> Victor,
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|