TECHNET Archives

November 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Chuck Brummer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Chuck Brummer <[log in to unmask]>
Date:
Wed, 11 Nov 2015 20:17:17 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Steve,

Appears that the lamination of DFSM has forced the SM into the holes.  If the spray pressure at develop is not adequate it will not clear the mask from the barrels.
Suggest you tell you supplier that this is a problem even if you do not reject the parts.  They can rework easily if they mask is not cured.
If I am incorrect, this is screened mask (of your you images looks very much like dry film, the other seems a little rough and might be liquid) they are spraying mask when the screen "snaps off" and contaminates the pad.

Based on your need you are making a good decision but I would still give feedback to the board supplier.


Chuck Brummer 
Medical Flex, EMSD
8357 Canoga Ave, Canoga Park, CA 91304-2605
Office: +1 818 734-4930 | Mobile: +1 805 890-8452
[log in to unmask]



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, November 10, 2015 10:32 AM
To: [log in to unmask]
Subject: [EXTERNAL] [TN] Unusual solder mask defect...

Hi All,

We just ran across a soldermask defect that I'm having trouble trying to figure out how it may have been caused. We build a .093" thick 8-layer assembly for a customer that is pretty picky as far as barrel fill is concerned. So we started noticing a problem on one lead of a component that we kept seeing no top solder fillet on that usually didn't have a problem.
Upon further investigation we saw that there was a solder mask ring down inside the barrel:

http://stevezeva.homestead.com/Soldermask_plug.jpg

So then I pulled the bare boards that we had in stock and found this:

http://stevezeva.homestead.com/Soldermask_plug_2.jpg

I would say that at least 2/3rds of the boards I looked at had this problem. What's kind of weird is that this mask ring would appear at the top of the barrel and sometimes at the bottom, but always the same hole.
The mask is an LPI, and what I'm having a hard time understanding is that the mask seems so well imaged around circumference of the pad, how does it get cured inside the barrel like that? And why is the ring sometimes at the top of the barrel and others down at the bottom?

I was able to clear the plug by carefully using a .033" drill bit under a microscope so that I didn't damage anything else in the barrel. I double checked the gerbers and there are no inner layer connections, the only connection is the trace that you see on the outer layer in the photo.
Because of time constraints we could not send the boards back to the fab vendor (even though I wanted to), but we put the next shipment on hold until they inspected for the problem. Why doesn't it surprise me that they said that they didn't see the problem? Sheesh...

So I'm just trying to understand what in the process could have caused this, a scratch in the artwork maybe?

Steve

-- 


This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original. 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
3M security scanners have not detected any malicious content in this message.

To report this email as SPAM, please forward it to [log in to unmask]

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2