TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Thu, 9 Sep 1999 12:25:20 +1000
MIME-Version:
1.0
X-To:
"Vandendolder, Ron" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (66 lines)
Ron, only one way to know :
solder both alloys in identical process on identical substrates/pads, etc.
any variations of cooling profile (just to mention something)
will influence readings on crystal formations = strength .
Answers are infinite, variable, customizable, ..............>>>>>

Hook your trusty puller on it ; compare :
you'll be home in one day with full validational base ;
spending one more day on documentation .

Beauty and shear strengths are only and always in the eye of the beholder
(As Werner may tell you as well ; if he digs himself out of his favorite
sandbunker)

Paul Klasek
ResMed

-----Original Message-----
From: Vandendolder, Ron [mailto:[log in to unmask]]
Sent: Wednesday, 8 September 1999 23:43
To: [log in to unmask]
Subject: [TN] acceptable solder joint shear strength?


Does anyone know what the minimum acceptable solder joint shear strengths
are for Sn63/Pb37 and In50/Pb50 ?

We are trying to optimize our soldering to gold interconnect process and
need some baseline/ industry standard numbers.

Thanks

Ron VandenDolder
Operations Manager
Millitech Corp
[log in to unmask]

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2