TECHNET Archives

December 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Tue, 16 Dec 2003 07:34:58 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=us-ascii
Subject:
From:
Reuven ROKAH <[log in to unmask]>
X-cc:
MIME-Version:
1.0
Parts/Attachments:
text/plain (222 lines)
Thanks Brian.

There is any hazards / risks during the process or rework (no cleaning is
possible only heating by solder iron?) such fumes from the solder iron?

Best  Regards

ROKAH Reuven

e mail: [log in to unmask]



                      Brian Ellis
                      <b_ellis@PROTONI         To:      [log in to unmask]
                      QUE.COM>                 cc:
                      Sent by: TechNet         Subject: Re: [TN] Conformal coating - PARYLENE DIMER DPX-C
                      <[log in to unmask]
                      >


                      15/12/2003 18:40
                      Please respond
                      to "TechNet
                      E-Mail Forum.";
                      Please respond
                      to Brian Ellis





By far the best protection of any kind of coating
Very uniform thickness, even over sharp edges and points
The vacuum/plasma reduces residual surface contamination, especially
hygroscopic volatiles
A bugger for rework
Expensive
GREAT!

Brian

Reuven ROKAH wrote:
> Hi Perylene users,
>
> Can you share with your experience and inform the + and - of this
process?
>
> I have last week visited one of the users site and it seems promising.
>
> I have long experience with spraying systems and not vacuum systems.
>
> Best  Regards
>
>  Reuven
>
>
>
>
>                       Graham Naisbitt
>                       <Graham.Naisbitt@CON         To:
[log in to unmask]
>                       COAT.CO.UK>                  cc:
>                       Sent by: TechNet             Subject: Re: [TN]
Foreign material on top of the conformal coating
>                       <[log in to unmask]>
>
>
>                       12/12/2003 18:02
>                       Please respond to
>                       "TechNet E-Mail
>                       Forum."; Please
>                       respond to Graham
>                       Naisbitt
>
>
>
>
>
> Bruce
>
> If you are applying epoxies and other materials after conformal coating,
> just be sure that the solvents (if any) are not affecting the coating
> during
> their application and curing.
>
> Otherwise this should simply be regarded as a cosmetic issue.
>
> Cleaning after all these processes is unlikely to be a good option, as
the
> coating will now be expected to withstand your cleaning process...and
> surface cleaning using brushes, swabs etc., are only likely to be moving
> the
> stuff around on the surface rather than removing it.
>
> Hope this helps
> --
> Regards Graham Naisbitt
>
> [log in to unmask]
>
> Cell: 079 6858 2121
> Office: +44 (0)1252 813706
>
> Concoat Limited - Engineering Reliability in Electronics
>
> NEW - HumiSeal 1H2O Bov Aerosol - NEW
>
> Web: www.concoat.co.uk  and  www.concoatsystems.com
>
>
>
>>Hey guys,
>>   I have be hit recently on a couple of occasions by the quality folks
>>over "foreign material" that is present on CCA's after conformal coating.
>>On quite a few boards we install heat sinks after CC and usually use an
>>epoxy to aid in heat transfer as well as loctite on the mounting screws.
>
> I
>
>>have been gigged for the residuals (just smears really) whether it is on
>>the solder pads or not.  I know that we all are concerned with material
>>left over directly on the solder connections, but I am having trouble
>
> with
>
>>this one from a logical standpoint.  I mean lets face it, you definitely
>>can't test for the presence of ionic contaminants or anything, but I know
>>the general impression is the boards should be clean.
>>
>>I know the simple answer here is to clean up all the residuals (and
>>everyone is instructed to do that), but there are times when stuff just
>>happens.
>>
>>Your thoughts
>>
>>Bruce Stilmack
>>GDLS-TO Manufacturing Engineer
>>(850) 574-4773
>>[log in to unmask]
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to
>>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at:
>
> http://listserv.ipc.org/archives
>
>>Please visit IPC web site
>
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>
>>additional information, or contact Keach Sasamori at [log in to unmask] or
>>847-509-9700 ext.5315
>>-----------------------------------------------------
>>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask]
or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2