TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
David Fish <[log in to unmask]>
Date:
Tue, 7 Nov 2000 06:22:26 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Franklin D Asbell <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Interesting comments...taking it a bit further, why not stick with
HASL...it is by far the less expensive of the more prominent finishes.

Yes, the OSP process is the easiest to maintain for the fabricator;
however, this finish does not provide for much flexibility to the
assembler, i.e. thermal cycles, risk of contamination, etc. The
immersion tin solves a few of these by increased thermal cycles in
comparison to OSP as well as providing a surface prior to wave/uv solder
that is more forgiving of contaminates found in even the most spot-free
assembly shop. Just those two conditions alone make the immersion tin a
more attractive finish over OSP.

Actually, when the process is well maintained, immersion tin is not much
more costly to the fabricator or the assembler...again, when it is well
maintained and in control.

Franklin

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------