TECHNET Archives

April 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Elstgeest Sander <[log in to unmask]>
Date:
Fri, 17 Apr 1998 17:28:06 +0000
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Elstgeest Sander <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Hello Technetters,

We are going to buy a PCB-prototyping mill, but we have been told that the
plating process with a special paste (as used by various manufacturers) is not
100% reliable. Therefore we are looking for other ways to create good via's. We
want via's with just a few (tens) of milliohms resistance, and we are looking
for an environmentally friendly and simple (preferably one bath) solution. The
size of the PCB's will be max. approx. 22 x 11 cm (8.6 x 4.3 inch).

Does anyone have any experience/advice for in-house plating solutions?

Sander Elstgeest
design engineer
NKF Electronics

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2