Victor
1) All plating systems have the aim of maintaining a surface with oxide layers that can be easily removed during the soldering operation. For that reason copper has to be kept protected from oxygen. One plating is nickel- gold. There are two problems associated with this system:
- Nickel forms a very stable oxide layer
- Gold reacts fast with copper even at room temperature and forms intermetallic layers that are not solderable.
This means, you are protecting the copper with gold but you need a barrier layer of nickel between the gold and the copper.
2) There is no necessity to use gold when you plate copper with a tin- alloy. The flux of the solder materials is designed to break down the tin oxide. Besides, gold dissolver very fast in tin and a gold plating would be eaten away during the tin plating process
3) Actually I am not aware of a reason for that. One reason might be to prevent the formation of tin-copper intermetallics during the plating process. Another reason could be that the copper surface was originally nickel- gold plated and re-tinned later on.
Best regards
Guenter
EMPA
Swiss Federal Institute for Materials Testing and Research
Centre for Reliability
Guenter Grossmann, Senior Engineer
8600 Duebendorf
Switzerland
Phone: xx41 1 823 4279
Fax : xx41 1823 4054
mail: [log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|