No, I mean applying solder to the iron, and then transferring it to the joint.
Ben
From: David Hillman [mailto:[log in to unmask]]
Sent: Wednesday, April 08, 2015 9:45 AM
To: TechNet E-Mail Forum; Gumpert, Ben
Subject: EXTERNAL: Re: [TN] Transfer Soldering
Ben - do you mean dippable solder paste?
Dave Hillman
Rockwell Collins
[log in to unmask]<mailto:[log in to unmask]>
On Wed, Apr 8, 2015 at 8:40 AM, Gumpert, Ben <[log in to unmask]<mailto:[log in to unmask]>> wrote:
Technetters,
Anyone have comments on transfer soldering?
It's identified in an IPC video as one of the seven sins of soldering, but seems to be focused on non-visible joints like through hole, as opposed to SMT or wire soldering.
There was a paper mentioned on Technet a while back which claimed transfer soldering was just as good as 'normal' soldering, but there was just a link to the abstract.
Ben
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|