TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Date:
Mon, 28 Jan 2008 20:02:38 +0200
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Gabriela Bogdan <[log in to unmask]>
Content-type:
text/plain; format=flowed; charset=iso-8859-1; reply-type=original
Subject:
From:
Gabriela Bogdan <[log in to unmask]>
Content-transfer-encoding:
7BIT
Parts/Attachments:
text/plain (84 lines)
Issues I read of was the surface roughness of the copper, and the thickness 
of the deposit.
Are these maybe factors to be checked and improved by the circuit suppliers?
Gaby
----- Original Message ----- 
From: "R Sedlak" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, January 28, 2008 7:51 PM
Subject: Re: [TN] Microvoids immersion silver


> Gaby:  Perhaps the ideal process to minimize/eliminate microvoids is one 
> that is almost unknown.   One of the more common issues in this process 
> can be marginal developing of soldermask, which leaves residues on pads. 
> Other than the obvious move, of keeping the developer in good condition 
> (not necessarily so easy, soldermask developers are very difficult to 
> clean out properly), the other insurance operation that can be done is to 
> put an alkaline cleaner before the microetch which precedes the silver 
> bath.
>
> This last suggestion should generate howls of protest, as everyone thinks 
> that alkaliine cleaners strip soldermask... to which I can reply, not ALL 
> of them do that.  There are alkaline cleaners specifically designed to 
> clean Copper, and leave soldermask unaffected.
>
> Good luck,
> Rudy Sedlak
> RD Chemical Company
>
> Gabriela Bogdan <[log in to unmask]> wrote: Dear Netters,
> Is there a preferred process for immersion silver finish in order to 
> minimize microvoids?
> How do you choose the preferred immersion silver PCB supplier?
> Which test for bare boards could give the best information?
> Should I perform a print and reflow test for each batch, followed by 
> x-ray?
> Which tests are the suppliers performing?
> Thanks,
> Gaby
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
> ---------------------------------
> Never miss a thing.   Make Yahoo your homepage.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2