TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 13 Sep 2011 20:13:58 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steven Creswick <[log in to unmask]>
Message-ID:
Subject:
From:
Steven Creswick <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (75 lines)
Blair,

As a follow-up on the commercial refrigerators, you can look at the following to get an idea of what I was attempting to describe.  I just searched for "commercial refrigerators"

http://www.missionrs.com/GDM-41SL-54.html

http://www.consolidatedfoodservice.com/true-gdm-49/

Typically, you can easily line the shelves with SS flat stock, and/or install vertical separators between vertical shelves to keep your reels upright.  Connect your own ESD measures, and/or blow incoming gas through an ionizer at the inlet.


Steve Creswick
http://www.linkedin.com/in/stevencreswick






-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair Hogg
Sent: Tuesday, September 13, 2011 4:26 PM
To: [log in to unmask]
Subject: Re: [TN] Dry Cabinets

Storage of MSDs, bare boards. 

On Tue, 13 Sep 2011 16:16:26 -0400, Joyce Koo <[log in to unmask]> wrote:

>What you try to use it for?
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair Hogg
>Sent: Tuesday, September 13, 2011 4:14 PM
>To: [log in to unmask]
>Subject: [TN] Dry Cabinets
>
>Howdy Technetters,
>
>Considering using dry cabinets as opposed to resealing MSD bags with fresh dessicant every time, oes anyone have good or bad experience with this?
>
>I've seen two types of dry cabinets, those that run with a continuous flow of dry nitrogen, and those that use dessicant packs which are periodically purged through a heating process. I found the second type online from companies like Totech and McDry/ Seika. 
>
>If you use dry cabinets, do they work well, and which type / manufacturer do you use? 
>
>Thanks,
>
>Blair

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2