What I mean is precondition. Not hand solder. As I mentioned before, you might need your component vendor's app note to find out the condition. LED for example.
--------------------------
Sent using BlackBerry
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Sunday, September 23, 2012 05:25 PM
To: TechNet E-Mail Forum <[log in to unmask]>; Joyce Koo
Cc: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] IPC Standard Temperature Profile for RoHS Pb Free Solder (Hand Soldering)?
Hi Joyce - neither one of these documents is a "standardized industry manual soldering profile" as such a creature does not exist. There are a number of factors that influence the temperature profile of a manual soldering operation. I think Dick is looking for something like we find in JSTD-033 but we don't have a typical temperature profile for a manual soldering process that I am aware of in the specifications.
Dave
Joyce Koo <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/21/2012 11:13 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Joyce Koo <[log in to unmask]>
To
<[log in to unmask]>
cc
Subject
Re: [TN] IPC Standard Temperature Profile for RoHS Pb Free Solder (Hand Soldering)?
http://www.minicircuits.com/app/AN60-031.pdf
http://www.avagotech.com/docs/AV02-0335EN
Joyce Koo
Materials Researcher - Materials Interconnect Lab
Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Linda Langley
Sent: Friday, September 21, 2012 10:56 AM
To: [log in to unmask]
Subject: Re: [TN] IPC Standard Temperature Profile for RoHS Pb Free Solder (Hand Soldering)?
Since the wrong temperature can be our worst nightmare, I would do a temp test starting with the lowest and increasing until I had the proper temp to do the job. I have always done this when there is no temp documented to go by. The proper size tip is also very important.
Linda Langley CIT
Training Specialist
248.829.4697
fax 248.853.6698
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: Friday, September 21, 2012 8:45 AM
To: [log in to unmask]
Subject: Re: [TN] IPC Standard Temperature Profile for RoHS Pb Free Solder (Hand Soldering)?
No, an optimized time-temperature profile depends on many factors, the
solder paste formula, the board laminate, the components on the assembly . .
.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard D. Krug
Sent: Friday, September 21, 2012 8:35 AM
To: [log in to unmask]
Subject: [TN] IPC Standard Temperature Profile for RoHS Pb Free Solder (Hand
Soldering)?
A customer has asked whether IPC has a standard temperature profile for RoHS
Pb-Free hand soldering. I'm not aware of one and since there are multiple
RoHS compliant alloys I don't know whether there should or could be one.
Is there any such document or series of documents?
Dick Krug, CSSBB, CSMTPE
Senior Process Engineer
Sparton Complex Systems
30167 Power Line Road
Brooksville, FL 34602-8299
p (352) 540-4012 (Internal Ext. 2012)
[log in to unmask]
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|