Blair
I would agree with Rudy. GC-MS will give you more information than IC
testing. We see these issues when alcohol is used to brush clean areas nearby. The
shinny film is most likely an organic or even a release agent in packaging
or handling issues.
In a message dated 2/21/2008 4:37:00 P.M. Eastern Standard Time,
[log in to unmask] writes:
Blair: My suspicion is that IC will tell you essentially nothing. From the
sound of your highly technical description, I would bet the residue is
largely organic, and most organics do not ionize, so IC would tell you little.
It MIGHT be flux residue, what sort are they using?
Would recommend trying to dissolve the residue in a solvent, and send out
for GC-Mass spec.
Even an elemental analysis would give you a direction to move in.
Rudy Sedlak
RD Chemical Company
Blair Hogg <[log in to unmask]> wrote: We are having an issues with
printed circuit boards showing residues,
that become more prevalent after heating cycles. It leaves a shiny / oily
looking film that is somewhat splotchy. Sorry for all these technical
terms.
I'm suspecting undercured epoxy, and I am currently looking to send
some out for chemical analysis. I have one lab quoting IC, and another's
website also recommends FT-IR. The supplier performed a ROSE test
and says there is no ionic contamination. The biggest problem we are
having is with conformal coating adherance. Due to certain components
on the one board that gives us trouble we aren't able to run it trhough
our aqueous wash cycle.
Is Ion Chromatography the right test? Any other suggestions?
Thanks,
Blair
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
Looking for last minute shopping deals? Find them fast with Yahoo! Search.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
**************Ideas to please picky eaters. Watch video on AOL Living.
(http://living.aol.com/video/how-to-please-your-picky-eater/rachel-campos-duffy/
2050827?NCID=aolcmp00300000002598)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|