TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Tue, 7 Oct 1997 12:59:59 -0400
Reply-To:
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
Organization:
Aydin Electro-Fab
From:
Art Shuler <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
Does anyone know of a way to completely eliminate gold slivers on a PWB
which is manufactured using a selective gold process? We realize due to
the etch factor, that there will be a 1.4 mil outgrowth when etching 1
oz. copper cladded material.

Mil-P-55110 recognizes that outgrowth will be present on conductors
plated with metals other than solder, but our customer cannot tolerate
slivering.  We've tried brushing them off with a brass wire brush, but
this seems to aggravate the problem.

Any input would be greatly appreciated.

Thank you

Art

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2