Brian,
Typically you would show a sideview of a 4 layer construction on your drawing. If you have any critical dielectric requirements between layers you should specify that. Also you should specify your finished copper weight requirements.
Hope this helps.
Ed Cosper
Director Quality Assurance and Engineering
Graphic Electronics inc.
----------
From: Brian Gaynor
Sent: Wednesday, October 07, 1998 10:00 AM
To: [log in to unmask]
Subject: [TN] (fab) Specify Multilayer Build
Hi technet readers,
What details are required when specifying the inner layer build of a
typical 4 layer multi (0.062" thick)?
If you state "make me a 4 layer board" what would you expect to
receive?
Best regards,
Brian Gaynor
Ireland
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|