TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Chuck Brummer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 3 Sep 2009 13:06:31 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (80 lines)
Jim.

Aside from the spec, pictures 1 & 3 don't bother me much as there is still 
a dam.  Picture 2 on the other hand looks like it could easily be broken 
off removing any barrier at all.

Assuming this to be photo imaginable?  I suspect we spent a little bit to 
much time in the developer.  Possible underexposed but probably to much 
develop.

Chuck Brummer
3M Manufacturing Engineer
8357 Canoga Ave.
Canoga Park, CA 91304-2605
(818) 734-4930




From:
J W <[log in to unmask]>
To:
[log in to unmask]
Date:
09/03/2009 12:55 PM
Subject:
[TN] Acceptability of Printed Boards (Solder Mask)
Sent by:
TechNet <[log in to unmask]>



Hello All,

Can someone point me to the section (s) in either IPC-6012 or IPC-A-600 or
other standards that explains the acceptance criteria for Solder Mask
UNDER-CUTTING?  Please go to Steve's web-site following the links below to
see a few pictures of a Solder Mask defect that was discovered by our
customer (they only stated "reject due to severe undercutting").  With 
this
situation, we are trying to help our China source fix this issue, and we
need to help them understand what section (s) of the standard (s) they
should be looking at so they can establish a corrective action.
http://stevezeva.homestead.com/files/Solder_Mask_Undercutting.jpg

http://stevezeva.homestead.com/files/Solder_Mask_Undercutting_2.jpg

http://stevezeva.homestead.com/files/Solder_Mask_Undercutting_3.jpg


Thanks,
Jim

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2