Louis,
Looks like that means a crack that crosses the thermal zone boundary (part in the thermal zone and part not). Similar to the location of "3" in Figure 3-15.
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Louis Hart
Sent: Friday, November 13, 2015 9:30 AM
To: [log in to unmask]
Subject: EXTERNAL: [TN] boundary line cracks
Technetters, IPC-6013C, 3.6.2.4, refers to 'boundary line cracks'. I do not find this term in IPC-T-50. What does it mean? Louis Hart
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|