Sadly, Joe, this is not the case. The consumer believes that lead in solder
is environmentally bad, and ultimately it's their buying power which makes
the decision.

Peter
--
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
Peter Swanson                                      Oxfordshire, England
Dynamix Technology Ltd
IPC Standards, Guidelines & Videos - Electronics Manufacturing Bookshop
[log in to unmask]    http://www.dynamixtechnology.com
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

-----Original Message-----
From: Joe Fjelstad [mailto:[log in to unmask]]
Sent: 17 February 2004 19:45
To: [log in to unmask]
Subject: Re: [TN] Another view of lead-free


In a message dated 2/17/2004 11:25:32 AM Pacific Standard Time,
[log in to unmask] writes:


> And yes, we all pretty much know that banning lead from electronics
assembly
> will do more environmental harm than good;

Hi Peter,

It seems that just about everyone knows this except for the EU Parliament...
;-)

Kind regards,
Joe

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2