TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Hogue, Pat (AZ76)" <[log in to unmask]>
Date:
Fri, 16 Apr 1999 13:29:05 -0700
MIME-Version:
1.0
X-To:
"Kasprzak, Bill (esd) US" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Hogue, Pat (AZ76)" <[log in to unmask]>
Parts/Attachments:
text/plain (68 lines)
NASA-STD-8739.3 dated December 1997 replaces NHB5300.4(3A-2).  Good luck.

Patrick Hogue
Materials and Processes Engineering
Honeywell Satellite Systems Operation
Glendale, AZ
(602) 561-3748
[log in to unmask]

> ----------
> From:         Kasprzak, Bill (esd) US[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;Kasprzak, Bill (esd) US
> Sent:         Friday, April 16, 1999 9:24 AM
> To:   [log in to unmask]
> Subject:      [TN] : New Revision of NHB5300.4(3A-2)
>
> Fellow tech-net readers:
>
> Does anybody know if the NASA soldering spec NHB5300.4(3A-2), dated  1992
> is
> going to be revised ? In many different ways it is behind the times.
>
> One area of my concern is the limited number of solvents that can be used
> according to paragraph 3A312 of this document. Most of the materials
> listed
> are Ozone Depleting Chemicals, which are more or less banned. We're using
> isopropyl alcohol.
>
> Has anyone working to this spec gotten any different materials for
> cleaning
> flux, approved by NASA?
>
> Anyone out there using FluxoffCZ, from Chemtronics, for any applications?
>
> Please respond through the net or if you prefer, directly to me at
> [log in to unmask]
>
> Thanks,
> Bill Kasprzak
> Moog Inc.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2