TECHNET Archives

February 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
IPC TechNet <[log in to unmask]>
Date:
Mon, 20 Feb 2006 10:53:25 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Content-type:
text/plain; charset="US-ASCII"
Subject:
From:
Graham Naisbitt <[log in to unmask]>
In-Reply-To:
Content-transfer-encoding:
7bit
Mime-version:
1.0
Parts/Attachments:
text/plain (180 lines)
You might also check every year the condition of the exhaust duct - it will
be liberally coated and that will have reduced the exhaust efficiency -
over-engineer, over-engineer, over-engineer....

Graham Naisbitt


On 16/2/06 16:01, "Douglas O. Pauls" <[log in to unmask]> wrote:

> Amol,
> In my opinion, "Zero Emissions" exists only in the minds of regulators and
> salesmen.  What they are talking about is a positive air flow spray booth
> that sucks all VOCs into one air stream.  That air stream becomes
> subsequently filtered, usually through a charcoal medium, such that any
> exhaust from the filter contains no VOCs or other regulated emissions.  If
> your spray booth exhaust is not filtered, even if properly permitted, then
> it has emissions.
>
> Doug Pauls
> Rockwell Collins
>
>
>
>
>              "Kane, Amol
>              (349)"
>              <akane@HARVARDGRP                                          To
>              .COM>                     [log in to unmask]
>              Sent by: TechNet                                           cc
>              <[log in to unmask]>
>                                                                    Subject
>                                        [TN] Zero Emissions Spray Booth
>              02/16/2006 08:11
>              AM
>
>
>              Please respond to
>               TechNet E-Mail
>                    Forum
>              <[log in to unmask]>
>              ; Please respond
>                     to
>                 "Kane, Amol
>                   (349)"
>              <akane@HARVARDGRP
>                    .COM>
>
>
>
>
>
>
> Dear TechNetters,
> A question was recently asked by a customer whether we have a "Zero
> Emissions Spray Booth" for conformal coating applications. We spray
> polyurethane, acrylic, epoxy and silicon coatings. We have an exhaust type
> spray booth to remove harmful vapors from the coating room. Can anyone shed
> some light on the Zero Emissions Spray Booth concept so that I can evaluate
> our existing infrastructure against the requirements and make upgrades if
> necessary.
>
> Thanks in advance,
>
> Amol Kane
> M.S (Industrial Eng.)
> Process Engineer
> Harvard Custom Manufacturing
> 941 Route 38  Owego, NY 13827
> Phone: (607) 687-7669 x349
> [log in to unmask]
>
>  -----Original Message-----
> From:   TechNet [mailto:[log in to unmask]]  On Behalf Of Dehoyos, Ramon
> Sent:   Thursday, February 16, 2006 8:33 AM
> To:     [log in to unmask]
> Subject:        Re: [TN] BGA Reflow profile - Thermocouples
>
>         Hi Dominic:
>         It should not cost you much to find out what is the temperature
> of a board through reflow. The investment of buying a Mole or other
> similar device, that will allow you to record the profile of a board
> through an oven is only "once". If you are using eutectic solder and
> your coldest components sees 20 degrees over the melting point which is
> 203 C  and you are not exceeding the highest temp that the most
> sensitive component may withstand, then you have a working profile, that
> simple.
>         Regards,
>         Ramon
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Dominic Boudreau
> Sent: Wednesday, February 15, 2006 5:50 PM
> To: [log in to unmask]
> Subject: [TN] BGA Reflow profile - Thermocouples
>
> Hello Techneter's,
>
> I am working on a procedure to make the reflow profile of a PCB.
>
> What are the techniques to know where to attach the thermocouples on the
> "PCB"? I already know that it should be where we have the coldest and
> hottest spot but is it possible to know when we "must" test a BGA to
> have a better reflow profile. We are a little company so we don't have
> the money to test a BGA each time we have one on a PCB.
>
>
>
> Thank you
>
>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2