We have used 2 part 5 minute epoxy without testing and without anyone checking into the material. We do not use a coating such as acrylic and silicon conformal like Regan Zintel mentioned in his note.

Has anyone heard good or bad about this.

Thanks for any assistance.
Wayne Bagwell
[log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2