TECHNET Archives

January 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Douglas Pauls <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 12 Jan 2012 15:17:02 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (109 lines)
The kindergarten factoid surprises no one, absolutely no one........

Doug Pauls



"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/12/2012 02:37 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Whittaker, Dewey (EHCOE)"      <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
Re: [TN] Hand Wipes and Lead Residues






Don't you find it strange that the man who is the icon for caramelized
corn refers to you as crackerjack? You're right about kindergarten; I got
detention even then for telling jokes during recess.
Dewey


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Thursday, January 12, 2012 1:18 PM
To: [log in to unmask]
Subject: Re: [TN] Hand Wipes and Lead Residues

Hi Doug - whomever said we learned everything we needed to know in life in

kindergarten was correct - including using soap when we wash our hands!
There are oodles (aka many) things in soaps that lead loves to grab onto
and make stable compounds. If people follow the prescribed practices for
correctly  handling solder/lead and use proper  hand washing practices,
then the need to hand wipes is not necessary.

Dave
crackerjack metallurgist presently hiding in Buffalo NY airport terminal





Douglas Pauls <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/12/2012 10:03 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
<[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] Hand Wipes and Lead Residues






Good morning all,

I just had a chat with one of our ES&H engineers, a very pleasent young
lady, on the topic of hand wipes and lead residues.  Was I aware of any
industry studies on the efficiency of hand wipes marketed at removing lead


residues, presumably from contact with cored wire solder?  I was not aware


of any.  I am always instantly suspicious of ANYTHING that marketers
touch.  I am of the opinion that good old fashioned hand washing with soap


and water is as effective as anything, but there are areas here where we
are pretty sure our operators go straight from the bench to lunch without
that step.

So, I turn to my favorite source of information.

1.  Are you aware of any industrial hygiene studies regarding
transferrence of lead to the hand, and/or the efficiency of "lead removal
wipes" in removing residues.
2.  In your facilities, do you use these kinds of wipes?
3.  If not, what measures do you normally use for operators cleaning hands


to remove potentially harmful material?

I will probably discuss this with our crackerjack metallurgist when he
returns from travel tomorrow, but thought I would ask in the mean time.

Doug Pauls