TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Rodney Miller <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Rodney Miller <[log in to unmask]>
Date:
Fri, 31 Mar 2006 08:31:53 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (42 lines)
Anyone, anyone, Bueller, Bueller....

I think this will work, but I'm interested if anyone has applied this to
PCB before?

-----Original Message-----
From: Rodney Miller [mailto:[log in to unmask]]
Sent: Wednesday, March 29, 2006 10:06 AM
To: 'TechNet '
Subject: Ultrasonic Weld to PCB with Ni Pads


I have a component with Nickel lead, a battery, and soldering/tinning it
has been troublesome.

I want to Ultrasonically Weld the leads to the PCB.  Can I do this with
PCB FR4 Material.  I was thinking if I cannot do it through the PCB
laminate, I might add a Via in pad and fill the via with Nickel plate.

The laminate is .030 and the finish option on the pads would be
Selective Immersion Ni, plated up to ???? 10um Maybe?

Any input appreciated....

Rodney L. Miller
Tri-onics Inc
Highland / Shanghai

Integrity and Solutions for Electronic Outsourcing



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2