Phil,
        rather than plating the through holes, why not fill with a screen
print/ thermal cure conductive? The effectiveness of this method may depend
on hole diameter & panel thickness.....
just a thought.

David Albin
Coates Circuit Products

-----Original Message-----
From: Phillip E. Hinton [mailto:[log in to unmask]]
Sent: 29 June 2001 05:45
To: [log in to unmask]
Subject: [TN] Copper Plating Aluminum


All

Some designer has called out a plated-thru PC board that has copper layers
and aluminum cores joined by plated thru copper holes.  I am aware of two
lousy methods that have been used.  One is to use electroless nickle instead
of electroless copper to give a metallic coating in the holes prep the
holes.
 A zincate process precedes the electroess nickel.  The second is to use a
board that has been zincated and use pryo copper asa a plating solution.

Does anybody have any other less difficult magical solution(s)

Thanks
Phil Hinton

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2