Hi Tom - 

	I can recommend using Indium CW-501, no-clean flux formulation with
SAC305 (indalloy 256).

	http://www.indium.com/products/circuitboardassembly/rework.php 

. Optimized for use with Sn/Pb and Pb-Free assembly
and rework processes
. Fast and excellent wetting to common Pb-Free
surface finishes including: ImmSn, ENIG, OSP
and ImmAg
. Minimal spattering & low odour
. Resistant to charring
. Reduced smoking
. Colophony-free

You can contact our USA HQ, based in Utica,NY

(P) 315 853 4900

Best Regards,
 
Graham Wilson
Applications Engineer

Indium Corporation of Europe


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tom P. Hummel
Sent: 08 October 2007 20:39
To: [log in to unmask]
Subject: [TN] RoHS wire solder

I have been assigned the task of getting samples of RoHS compliant wire
solder to evaluate.  I was wondering what brands and types of solder are
being used in the market.  Does anyone have a preference /
recommendation for RoHS wire solder?

 

Thomas P. Hummel

Carlton Industries Corp

[log in to unmask]

Phone  203-288-5605

Fax  203-288-9202

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited. 

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2