>>> Jason Williams <[log in to unmask]> 09/17/01 02:26PM >>>
Shredder,
First off, get rid of that oversized entry you mentioned. Get slightly
undersized entry and tape on two sides only.
Some questions you need to ask:
What has your drill supplier done to help?
What type of material and how many layers are you drilling?
Is the material fully cured?
Is there sufficient vaccuum?